Fe-Ni cores are excellent candidates for switching regulator inductors, transformers, reactors and in-line noise filters. Herein the influence of the phenol binder content on the microstructure and magnetic properties of Fe-50 wt% Ni powder cores in the high frequency range is investigated. Regardless of the binder content, all cores form a disordered A1 phase. The saturation magnetization (4πMs) and initial permeability increase as the binder content decreases. The core with a binder content of 0.5 wt% shows a relatively high 4πMs of 1.38 T and the highest permeability value of 70.9. Moreover, the total core loss (Pcv) with frequency ranges from 5 kHz to 1 MHz under a magnetic flux density of 10 mT depending on the binder content. A binder content of 3.0 wt% significantly reduces Pcv in the high frequency range above 100 kHz. At a frequency of 500 kHz, the Pcv values are 154.9, 128.7, and 133.8 kW/m3 for the cores with binder contents of 0.3, 0.5, and 1.0 wt%, respectively, but the value drastically decreases to 60.5 kW/m3 for a binder content of 3.0 wt%. Thus, the binder, which acts as an insulator layer between particles, affects the eddy current and consequently, Pcv. These results demonstrate that Fe-Ni powder cores exhibit excellent soft magnetic properties at various frequencies and suggest that a binder content of 3.0 wt% may realize optimal properties for future high frequency applications.
Year:
2024
Fe-based amorphous powder cores of Fe–Si–B–Cr–C magnetic powder and phenolic binder were fabricated, and the effects of annealing and compaction pressure on the soft magnetic properties and core loss were investigated. The formation of Fe–B and α-Fe (Si) phases was confirmed at the annealing temperature above 773 K. The density gradually increased from 5.3 to 5.5 g/cm3 as annealing temperature increased, resulting in the saturation magnetization 4πMs increased to 1.0 T at 773 K. The effect of compaction pressure was studied by using samples annealed at 723 K. Both the density and 4πMs enhanced with compaction pressure from 980 to 1960 MPa. The real part of permeability µ’ remained constant for the frequency up to 2 MHz. The initial value of µ’ increased from 25 to 38 with compaction pressure. Consequently, at Bm of 50 mT and frequency of 100 kHz, the considerably low core loss of 67 kW/m3 was obtained. The low core loss and moderately high permeability of Fe–Si–B–Cr–C amorphous powder core across a wide frequency range indicate its potential for application in high frequency electronic components.
Year:
2024
Year:
2023
Year:
2023
Collaborators (2)
Satoshi Okamoto
Professor
Tohoku University
Yasushi Endo
Professor
Tohoku University
Make your next move.
Prepare your application
Review drafts before you send them.