Accurate evaluation of iron loss in soft magnetic materials is often hindered by low signal-to-noise ratio (SNR) conditions, such as at low frequencies or in materials with low permeability. The conventional averaging method, which corresponds to ensemble averaging of repeated single-cycle waveforms, is effective for noise suppression but is time-consuming and susceptible to errors due to environmental drift, while filtering and frequency-domain denoising techniques improve SNR at the cost of waveform fidelity. We propose a Bayesian inference framework integrated with the two-coil method for physics-oriented analysis, which reconstructs current and voltage waveforms and directly provides amplitudes, phases, and noise levels together with credible intervals. Experimental validation demonstrated that the proposed approach achieves more reliable loss estimation with far fewer signal averages than the conventional methods. The framework provides a robust and efficient solution for magnetic-material characterization and has the potential to be extended beyond sinusoidal excitation to more complex excitation conditions in future studies.
Year:
2026
Fe-based amorphous powder cores of Fe–Si–B–Cr–C magnetic powder and phenolic binder were fabricated, and the effects of annealing and compaction pressure on the soft magnetic properties and core loss were investigated. The formation of Fe–B and α-Fe (Si) phases was confirmed at the annealing temperature above 773 K. The density gradually increased from 5.3 to 5.5 g/cm3 as annealing temperature increased, resulting in the saturation magnetization 4πMs increased to 1.0 T at 773 K. The effect of compaction pressure was studied by using samples annealed at 723 K. Both the density and 4πMs enhanced with compaction pressure from 980 to 1960 MPa. The real part of permeability µ’ remained constant for the frequency up to 2 MHz. The initial value of µ’ increased from 25 to 38 with compaction pressure. Consequently, at Bm of 50 mT and frequency of 100 kHz, the considerably low core loss of 67 kW/m3 was obtained. The low core loss and moderately high permeability of Fe–Si–B–Cr–C amorphous powder core across a wide frequency range indicate its potential for application in high frequency electronic components.
Year:
2024
Collaborators (2)
Mai Phuong Nguyen
Assistant Professor
Tohoku University
Yasushi Endo
Professor
Tohoku University
Make your next move.
Prepare your application
Review drafts before you send them.